Yea I only got chemical gloves and glasses. No HEV suit...
Happy to just get the 33%.
Printable View
Hmmmm Not looking great...
https://s1.postimg.cc/7wz5o4ht1b/IM..._155340523.jpg
Ill leave it in the dye for 15 mins and come back.
Great - glad we managed to dig to the bottom of the problem!
good job :)
Just want to check.
1L of 33% battery acid (I have 31-38%) mixed with 3L of water for 4.5asf?
Had the amazing, original idea of using one of these stone air things from fish tanks.
Have to say, works really well.
https://s9.postimg.cc/qjb2c891r/IMG..._204238780.jpg
https://media.giphy.com/media/1vZaA7...9avK/giphy.gif
https://media.giphy.com/media/8quBjt...OhA9/giphy.gif
Worked really well. The larger bubbles before sometimes caused me issues but this is great.
Not 100% there yet. More practice and experimenting me thinks.
https://s9.postimg.cc/r7oi8mmrz/IMG_..._235228049.jpg
Looking good.
Can I just ask - what are you using for your cathode? (I did start setting myself up for anodizing but a squirrel ran past and I moved onto something else)
Wow the result is very good, nice work!