And if you have not done it till now, do it - compressor, 0.6-0.8mm ID tube blowing air / or air plus cooling liquid/ right where the cut happens. Cooling things down tremendously affects bit life and finish result. later i will show you picture of my setup if you have not done yourself a mist cooler.