Quote Originally Posted by Tom J View Post
My frame was not more than 1mm warp as I tack it everything and weld one bead at the time, cool down and opposite side and so on. I have to admit that I broke my rule and did not let to cool enough (firstly was warp corners down than after cool opposite) - £100+ waste on steel and gas, lesson learnt. I bit it with sledge hammer, driven by the car and finally filled down, so my 8mm bars became 4mm in places:)
Now I use Tig just to see if I can do better
Click image for larger version. 

Name:	IMG_1256.jpg 
Views:	281 
Size:	280.5 KB 
ID:	20098Click image for larger version. 

Name:	IMG_1257.jpg 
Views:	293 
Size:	147.1 KB 
ID:	20099
TIG will give a better result but will still warp. Either way it can be a pickle when working with steel. I still haven't decided what bed to go with on mine. I will probably do MDF to start with.