Hi Spud

The link below is a PowerPoint presentation a while back, It details how I made an epoxy bearing material using epoxy, metal powder and some low friction materials. Teflon, molybdenum disulfide, and graphite, these three elements are not needed for an epoxy grout. You can make a thick paste from epoxy and iron powder alone that will make an excellent high strength grout for filling the small voids left between machine members.
As you live in Australia the sources at the end of the PowerPoint are relevant.

http://www.mediafire.com/file/022r26...mpact.ppt/file

The link below is to a great build done some time ago. The post clearly explains how the builder used epoxy to grout joints before bolting.

http://oneoceankayaks.com/madvac/madvac_index.htm

Hope this helps

Regards
John