Quote Originally Posted by ngwagwa View Post
The study you link to used conventional heating to normalize the material. They quote a time of 30 minutes at 870 °C but don't mention the cooling down rate or time.
The material comes annealed and i will machine it, so no stress here. Its oil quenched, oil at 40C