Quote Originally Posted by ecat View Post
Two big problems:
1) The cost of ali epoxy, http://uk.farnell.com/araldite/arald...0ml/dp/1759545, need to add in the cost of a dispensing gun too, I think.
2) The fact that even with surface prep the special epoxy is not a guaranteed strong, long lasting join.

Since all I'd be using the epoxy for is to make the filling between two lumps of metal is it necessary to use ali epoxy? And indeed, am I obsessing over trivial detail ?
Hopefully you shouldn't need much epoxy, where you need to fill anything over a few tenths of a mm you could put glass fibre cloth in the space. It will be better to use a thixotropic or fairly viscous variant than the west system stuff which is designed to wet out composites and is a pretty thin liquid. I don't think you need to worry too much about bonding if it's trapped in a clamped interface - using epoxy to actually make the join is another matter and you would need very good surface prep and glue / material selection in that case.

I've a length of 3" square 1/4" wall aluminium that I'm intending making my router out of but I haven't had chance to do any measuring on it. I'm hoping it will be close enough that I can just use a thin layer of epoxy on the interfaces and by initially clamping the rails down very lightly until the epoxy sets ensure that they are not deformed by the box section. It'll be at least a couple of months before I get to that stage so I'm looking forward to reading how you get on