    updated for you mate ;)
    my de-smut and pro dye (blue) came today will post when i have had a play :)
    there is no such thing as a stupid question, just stupid answers !!!!

  2. #2
    Have you tried any of the commercial dye yet? I think you'll find it a lot better.

    One thing I've found with anodising is that you need to clean stuff with distilled water, a LOT. Clean in with normal water, then distilled, then etch it, then clean again with distilled, then anodise in distilled water&acid, then clean in distilled water, then dye (with the dye made up with distilled water), then seal in distilled water.

    If you don't do that I've found you get nasty white deposits on the part.

    Here's the first part I anodised, 2 years ago now

    Click image for larger version. 

Name:	DSC02366_small.jpg 
Views:	947 
Size:	471.9 KB 
ID:	3707

Thread Information

Users Browsing this Thread

There are currently 3 users browsing this thread. (0 members and 3 guests)

Similar Threads

  1. Home is where the part is?
    By HankMcSpank in forum Machine Discussion
    Replies: 4
    Last Post: 15-07-2013, 09:58 AM
  2. WANTED: home built cnc
    By japcarmaniac in forum Items Wanted
    Replies: 1
    Last Post: 24-04-2013, 02:35 AM
  3. Home Anodising Aluminium and the elusive Sulphuric acid
    By GeorgeD in forum Metalwork Discussion
    Replies: 10
    Last Post: 01-02-2013, 03:07 PM
  4. value of home switches
    By engineshed in forum General Electronics
    Replies: 3
    Last Post: 04-04-2012, 12:01 AM
  5. Aluminium passivation - for aluminium to be used outside
    By CHudson in forum Metal Finishing Techniques
    Replies: 4
    Last Post: 06-04-2011, 09:18 PM

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •