20-05-2012 #1
It's an actual case, a home electronics plastic housing.
Please see below pictures:
-
21-05-2012 #2
improve product design, increase the hole as shown below.
injection molding surface ok!!
-
So you are saying the sliding component used to make the transverse hole had some spring in it and gave the kind of scuff mark usually associated with insufficient draft angle and a sparked finish?
I can see how the new hole would reduce the force springing the slide open, but somehow it doesn't look big enough???
-
22-05-2012 #4
Can you explain the point of this thread has I'm struggling to see it.??
-
22-05-2012 #5
Hi,all.
Perhaps this explanation as below picture, anyone can better understand.
Please see:
-
22-05-2012 #6
Hi, Robin . Yes, increase draft angle is a method. But this Product shape design is not allow the change of draft angle.
-
-
22-05-2012 #8
Thread Information
Users Browsing this Thread
There are currently 1 users browsing this thread. (0 members and 1 guests)
Similar Threads
-
Mould Examples
By gavztheouch in forum Moulding MachinesReplies: 3Last Post: 26-05-2014, 05:51 PM -
Mould polishing and texture advice
By dazza in forum Moulding MachinesReplies: 13Last Post: 26-01-2014, 10:06 AM -
RFQ: RFQ - choc mould
By cooliced in forum Projects, Jobs & RequestsReplies: 2Last Post: 18-10-2012, 10:50 AM -
Need advice on surface finish
By FatFreddie in forum Machine DiscussionReplies: 4Last Post: 01-05-2010, 02:51 PM
Bookmarks