Thread: Hard colour anodising
Threaded View
-
03-03-2013 #6
i was tempted to inject liquid butane into a part to keep the temperature low enough for hard anodising, not a wise option at all considering a slight knock on the hanger wires would blow the roof off the shed.... but perfectly ok for mad science purposes :)
Thread Information
Users Browsing this Thread
There are currently 1 users browsing this thread. (0 members and 1 guests)
Similar Threads
-
RFQ: CLOSED - Aluminium milling and anodising
By AlexTsekenis in forum Projects, Jobs & RequestsReplies: 0Last Post: 12-05-2014, 10:11 PM -
Anodising legalities
By m_c in forum Metal Finishing TechniquesReplies: 7Last Post: 07-01-2014, 08:42 PM -
RFQ: Why is it so hard...
By ktc in forum Projects, Jobs & RequestsReplies: 10Last Post: 11-08-2013, 08:05 PM -
Forum colour
By Rogue in forum General DiscussionReplies: 18Last Post: 11-08-2013, 06:50 PM -
Home Anodising Aluminium and the elusive Sulphuric acid
By GeorgeD in forum Metalwork DiscussionReplies: 10Last Post: 01-02-2013, 03:07 PM
Bookmarks