Quote Originally Posted by Clive S View Post
I found that a warm air gun flashed across the surface got rid of the bubbles. As a matter of interest the Wests System was still like thick water 6 or 7 hors after the pour before its started the cure. With no sticky stuff on the top when cured. Also the mixing was just done with a flat bit on thin ply and gently stirred it round. ..Clive
You mentioned this before so I tried a hair drier (it's the wife's, no use to me now) on it's lowest speed but it was moving the epoxy round like the seas at Cape Horn.
Yes I think this epoxy was still flexible after 6 to 7 hours but maybe just beyond any self leveling properties on the scale required.
It's interesting you confirm the slow mixing method.