    Trying to balance the flow with the shrinkage while it hardens sounds like a recipe for disaster.

    Pour, flow, cut off, harden!

    Cutting the rail into equal size/shape sections should give consistent shrinkage. If you do repeated bi-sections to cut the rail (eg into 4 or 8) then (with skill/slow cut) even the slight increase in pool height should be even in each pool.

    edit:
    More likely to work and easier: One big ring of equal cross section is the best answer. Ideally you would not have a 90deg corner near what will be the final end of the epoxy rail, a radius would be nice.

    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	epoxy.jpg 
Views:	2065 
Size:	107.2 KB 
ID:	13618  
    Last edited by jimbo_cnc; 15-10-2014 at 11:49 AM.

Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •