Threaded View

Previous Post Previous Post   Next Post Next Post
  1. #6
    Quote Originally Posted by m_c View Post
    I've always used soluble oil, and never had any issues with staining, however I am aware there are some that are notorius for causing residue build up.
    One big thing to be aware of is soluble oils can be pretty specific for their applications, and I'm guessing that whatever you have isn't suited for brass (some suppliers classify it as yellow metal).
    +1

    I use Castrol Cooledge BI, mainly because I got most of a 20L container cheaply. I've not needed to use it on brass, but it says it's suitable in the datasheet.
    Last edited by Jonathan; 11-05-2014 at 11:36 PM.
    Old router build log here. New router build log here. Lathe build log here.
    Electric motorbike project here.

Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

Similar Threads

  1. Coolant, I am not sure which one to go with.
    By suesi34e in forum Swarf & Chip Management
    Replies: 23
    Last Post: 17-10-2015, 07:13 PM
  2. My Coolant System
    By Tenson in forum Swarf & Chip Management
    Replies: 6
    Last Post: 08-04-2013, 01:59 PM
  3. coolant
    By luke11cnc in forum Machine Discussion
    Replies: 4
    Last Post: 11-02-2012, 01:17 PM
  4. What coolant to use??
    By don_jarr in forum General Discussion
    Replies: 13
    Last Post: 05-11-2011, 03:12 PM
  5. eBay: Castrol Cooledge Cutting Coolant Suds
    By Lee Roberts in forum Items On eBay UK
    Replies: 3
    Last Post: 09-08-2009, 09:42 PM

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •