~In the past, I have used melamine lacquer. The stuff I used dried very quickly and hardened over 24 hours (I think it absorbed carbon dioxide from the air as a catalytic hardener). When it had hardened it was super tough. I sprayed it with a high pressure gun, but in those days HVLP was not invented.