Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1
    D.C.'s Avatar
    Lives in Birmingham, United Kingdom. Last Activity: 05-01-2016 Has been a member for 9-10 years. Has a total post count of 326. Received thanks 30 times, giving thanks to others 24 times.
    Quote Originally Posted by Robin Hewitt View Post
    If all you want is to flow a flat surface, why not use Wood's Metal?
    Not a bad idea but Wood's Metal / Cerrobend etc looks to be about £40 per kg, so it would cost a lot more than epoxy levelling I think?
    Have you ever tried it if you have some lying around?

    Quote Originally Posted by Sven View Post
    I' ve been reading up on EG as my own ideas are taking shape.
    As far as I' read, vibrating EG does not work unless you use a mix with too much epoxy for a small size casting. Too much meaning it will yield an end result that has some shrinkage and maybe some warp.
    The best seems to be a mix that is "very dry" compared to what most people on forums seem to be using: in the 4% area, or a bit wetter where it needs to adhere to another material.
    Also, best to use various grain sizes, the next size 1/5th of the previous.
    Put a measured amount in a jar, then add the smaller size and shake until the volume increases and you know the ratio.
    A dry mix like that will need stamping.
    And off course, make sure to do trials :)
    For larger aggregate This place does washed, graded and dried quartz specifically for resin bonding:
    http://resinbondedaggregates.com/cat...ound-aggregate

    For the smaller sizes I think it would have to be blasting grits:
    http://www.stacey-processing.com/gla...ing-media.html

    Then Aluminium Oxide powder and milled CF.

  2. #2

  3. The Following User Says Thank You to Robin Hewitt For This Useful Post:


  4. #3
    Sven's Avatar
    Lives in a, Netherlands. Last Activity: 07-05-2020 Has been a member for 9-10 years. Has a total post count of 46. Received thanks 4 times, giving thanks to others 0 times.
    I may have had my expansion reasons mixed up...

    A guy I know built an epoxy-concrete machine with steel bars at the surface to connect the rails to.
    They were flat when casting started but the end result was not.

    If you cast EC in a steel tub, it may end up not being part of the construction but just a liner and not a reinforcement.

  5. #4
    There are many ways to not do it right. Apart from choosing the best epoxy for deep casting, is good idea to read the documents of the said epoxy and follow them instructions to the letter. best is to call the epoxy manufacturer and speak with them for the most suitable epoxy for the purpose.

    Cause at the end of the day they know their stuff and even can mix a custom epoxy for your purpose. I have talked with one company technician and he knew exactly about that situation and explained me the differences between the 3 suitable epoxies they had.
    project 1 , 2, Dust Shoe ...

  6. #5
    D.C.'s Avatar
    Lives in Birmingham, United Kingdom. Last Activity: 05-01-2016 Has been a member for 9-10 years. Has a total post count of 326. Received thanks 30 times, giving thanks to others 24 times.
    The http://durcrete.de is quite interesting.

    What I was aiming for was finding a sweet spot between price/performance and ease of construction given that I only have not very accurate tools to work with.



    The Durcrete site has some vibration damping data available and a demo:
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	daten-schwingungsdaempfung.jpg 
Views:	606 
Size:	46.8 KB 
ID:	15902  

  7. #6
    Definitely they are the most promising ones. I remember spending 2 weeks of my free time / when i had one/ browsing and searching. And thinking of it its not at all so expensive as it could be with the epoxy. I had somewhere their offer and it was relatively cheap. from their site:

    Do It Yourself

    Durfill is a simple and quick solution. So we have a lot of clients all over Europe, which use this high strength grout for filling their machine components. Without additional dealers, we export the material in full palettes including the required delivery directly to your company.

    Last edited by Boyan Silyavski; 19-08-2015 at 09:19 AM.
    project 1 , 2, Dust Shoe ...

  8. The Following User Says Thank You to Boyan Silyavski For This Useful Post:


Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

Similar Threads

  1. Designing a Gantry type concert router
    By Jazmal in forum Gantry/Router Machines & Building
    Replies: 5
    Last Post: 09-01-2015, 05:52 PM
  2. Designing a Metal milling bushless Spindle
    By Kevman in forum Electronic Project Building
    Replies: 18
    Last Post: 14-04-2013, 06:43 PM
  3. A little help on designing in Solidworks
    By D-man in forum Computer Software
    Replies: 3
    Last Post: 04-11-2010, 10:49 PM
  4. Looking for some help designing my gantry please
    By psiron in forum Gantry/Router Machines & Building
    Replies: 13
    Last Post: 05-07-2010, 09:52 PM

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •