  1. #2
    A single flute or fast helix two flute cutter should work OK.
    Peck drill to control swarf length, a ramped internal strategy for your 3.5 holes and outlines should generate chips not continuous swarf, the best path for your 10mm will depend on the strategies available in your CAM,
    Regards,
    Nick
    Last edited by magicniner; 06-03-2016 at 02:03 PM.

  2. The Following User Says Thank You to magicniner For This Useful Post:


Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

Similar Threads

  1. RFQ: laser cut - very simple rectangular parts, PTFE and other flex plastics
    By dsc in forum Projects, Jobs & Requests
    Replies: 0
    Last Post: 19-06-2015, 12:59 AM
  2. PTFE coating small parts in the UK - one offs
    By dsc in forum Marketplace Discussion
    Replies: 0
    Last Post: 22-12-2013, 09:07 PM
  3. A suggestion on the forum rules
    By John S in forum General Discussion
    Replies: 2
    Last Post: 09-09-2012, 02:34 PM
  4. Suggestion.!! . . Am I the only one it BUGS.!!
    By JAZZCNC in forum General Discussion
    Replies: 2
    Last Post: 22-07-2012, 08:04 PM

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •